A SAW welding operator is attempting to quality by radiography on a 6 inch thick test coupon. Elongated slag inclusions are measured to be 0.2 inch long.
Must weld 2 additional coupons;
meets the requirements
slag must not exceed 0.5"
slag is not acceptable.